The effect of silver diamine fluoride in preventing in vitro primary coronal caries under pH-cycling conditions
Date
Language
Embargo Lift Date
Committee Members
Degree
Degree Year
Department
Grantor
Journal Title
Journal ISSN
Volume Title
Found At
Abstract
Objectives This study investigated the ability of SDF, and its individual components, silver (Ag+) and fluoride (F−) ions, in preventing enamel demineralization under pH-cycling conditions in the presence or absence of twice-daily fluoride application.
Design Polished human enamel specimens were assigned to five treatment groups (n = 36 per group): SDF (38 %); SDF followed by application of a saturated solution of potassium iodide (SDF + KI); silver nitrate (AgNO3; silver control, 253,900 ppm Ag); potassium fluoride (KF; fluoride control, 44,800 ppm F); deionized water. Treatments were applied once. Specimens in each treatment group were divided into two subgroups (n = 18). During the subsequent 7-day pH-cycling phase, specimens were treated twice daily with either 275 ppm fluoride as sodium fluoride or deionized water, immediately before and after a 3-h cariogenic challenge with exposure to artificial saliva at all other times. Changes in color, Vickers surface microhardness (SMH), transverse microradiography (TMR) was calculated. Data were analyzed using two-way ANOVA.
Results In both models, SDF, SDF + KI and KF were superior in inhibiting demineralization compared to AgNO3 and deionized water (p < 0.0001). There was no statistically significant difference between SDF, SDF + KI and KF with twice daily fluoride treatments (p > 0.8). However, KF was more effective in preventing demineralization than SDF and SDF + KI in the absence of fluoride treatments (p = 0.0002). KI did not affect the ability of SDF to prevent demineralization (p > 0.4).
Conclusion SDF and SDF + KI appears to be an effective option in preventing primary coronal caries.