Self-assembling peptide-laden electrospun scaffolds for guided mineralized tissue regeneration

dc.contributor.authorde Souza Araújo, Isaac J.
dc.contributor.authorFerreira, Jessica A.
dc.contributor.authorDaghrery, Arwa
dc.contributor.authorRibeiro, Juliana S.
dc.contributor.authorCastilho, Miguel
dc.contributor.authorPuppin-Rontani, Regina M.
dc.contributor.authorBottino, Marco C.
dc.contributor.departmentBiomedical and Applied Sciences, School of Dentistry
dc.date.accessioned2024-10-22T09:08:14Z
dc.date.available2024-10-22T09:08:14Z
dc.date.issued2022
dc.description.abstractObjectives: Electrospun scaffolds are a versatile biomaterial platform to mimic fibrillar structure of native tissues extracellular matrix, and facilitate the incorporation of biomolecules for regenerative therapies. Self-assembling peptide P11-4 has emerged as a promising strategy to induce mineralization; however, P11-4 application has been mostly addressed for early caries lesions repair on dental enamel. Here, to investigate P11-4's efficacy on bone regeneration, polymeric electrospun scaffolds were developed, and then distinct concentrations of P11-4 were physically adsorbed on the scaffolds. Methods: P11-4-laden and pristine (P11-4-free) electrospun scaffolds were immersed in simulated body fluid and mineral precipitation identified by SEM. Functional groups and crystalline phases were analyzed by FTIR and XRD, respectively. Cytocompatibility, mineralization, and gene expression assays were conducted using stem cells from human exfoliated deciduous teeth. To investigate P11-4-laden scaffolds potential to induce in vivo mineralization, an established rat calvaria critical-size defect model was used. Results: We successfully synthesized nanofibrous (∼ 500 nm fiber diameter) scaffolds and observed that functionalization with P11-4 did not affect the fibers' diameter. SEM images indicated mineral precipitation, while FTIR and XRD confirmed apatite-like formation and crystallization for P11-4-laden scaffolds. In addition, P11-4-laden scaffolds were cytocompatible, highly stimulated cell-mediated mineral deposition, and upregulated the expression of mineralization-related genes compared to pristine scaffolds. P11-4-laden scaffolds led to enhanced in vivo bone regeneration after 8 weeks compared to pristine PCL. Significance: Electrospun scaffolds functionalized with P11-4 are a promising strategy for inducing mineralized tissues regeneration in the craniomaxillofacial complex.
dc.eprint.versionAuthor's manuscript
dc.identifier.citationde Souza Araújo IJ, Ferreira JA, Daghrery A, et al. Self-assembling peptide-laden electrospun scaffolds for guided mineralized tissue regeneration. Dent Mater. 2022;38(11):1749-1762. doi:10.1016/j.dental.2022.09.011
dc.identifier.urihttps://hdl.handle.net/1805/44119
dc.language.isoen_US
dc.publisherElsevier
dc.relation.isversionof10.1016/j.dental.2022.09.011
dc.relation.journalDental Materials
dc.rightsPublisher Policy
dc.sourcePMC
dc.subjectBiomineralization
dc.subjectBone regeneration
dc.subjectElectrospinning
dc.subjectScaffolds
dc.subjectSelf-assembling peptide
dc.titleSelf-assembling peptide-laden electrospun scaffolds for guided mineralized tissue regeneration
dc.typeArticle
Files
Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
deSouzaAraújo2022SelfAssembling-AAM.pdf
Size:
4.3 MB
Format:
Adobe Portable Document Format
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
2.04 KB
Format:
Item-specific license agreed upon to submission
Description: